Key Features: – Efficient Oxide Removal: Rapidly removes aluminum surface oxide film at high temperature – Excellent Wettability: Significantly improves wetting and spreading of filler metal on base material – Wide Compatibility: Compatible with aluminum-silicon, zinc-aluminum, and various filler metals – Superior Thermal Conductivity: Brazed joints offer good thermal conductivity, suitable for heat exchange applications – Reliable Sealing: Excellent joint sealing, suitable for pressure vessels and piping systems
Technical Specifications: – Applicable Materials: Aluminum, aluminum alloys, aluminum-copper composites – Brazing Temperature Range: 580-620°C (depending on filler metal type) – Physical Form: Powder or paste – Active Temperature: Above 550°C
Applications: – Automotive radiator manufacturing – Air conditioning condenser and evaporator assembly – Heat exchanger and heat transfer equipment manufacturing – Aluminum piping system connections – Brazing of aluminum thin-walled containers and components
Usage Instructions: 1. Surface Preparation: Clean brazing area, ensure no oil or impurities 2. Apply Flux: Evenly apply flux at brazing joint 3. Place Filler Metal: Position filler metal at joint location 4. Heat for Brazing: Heat to brazing temperature, melt filler metal and fill joint 5. Cool and Clean: After natural cooling, remove residual flux
Packaging & Storage: – Package Specifications: 500g/bottle – Storage Conditions: Sealed storage in cool and dry place – Shelf Life: 18 months
Precautions: – Maintain good ventilation during use – Avoid inhaling fumes during heating process – Wear appropriate personal protective equipment – Thoroughly remove residual flux after brazing to prevent corrosion